Chemical Composition *Carbon and silicon targets are specified for each bar size in order to maintain mechanical properties. Small amounts of alloying elements are used to stabilize the pearlitic structure. Magnesium treatment is employed to produce nodular graphite.
| Carbon | 3.50 - 3.90% |
| Silicon | 2.25 - 3.00% |
| Manganese | 0.15 - 0.35% |
| Sulfur | 0.025% Max |
| Phosphorus | 0.05% Max |
Mechanical Properties Hardness properties for various diameters are shown in the table. Hardness properties listed are minimum and maximum across the bar. For rectangles, squares and shapes, the hardness properties will depend on minimum and maximum section thickness and will be supplied on request.
| 01.000 - 20.000 | 25 – 508 | 241 | 329 |
Tensile strength is determined from a longitudinal test specimen taken from mid-radius of the as-cast bar.
| Tensile strength psi (min) | 100,000 |
| Yield strength psi (min) | 70,000 |
| Elongation (min) | 3% |